Technical center

These corrosion data are mainly based on results of general corrosion laboratory tests, carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen).

All concentrations are given in weight-% and the solvent is water if nothing else is shown. The corrosion data apply to annealed materials with normal microstructure and clean surfaces, throughout.

Camphor
Temp. °C 20
Grade or type of alloy:
Carbon steel
13 Cr
Sandvik 1802
Sandvik 3R12
Sandvik 3R60
18Cr13Ni3Mo 1)
17Cr14Ni4Mo 2)
Sandvik 2RK65 ('904L')
Sanicro 28
254 SMO
654 SMO
Sandvik SAF 2304
Sandvik SAF 2205
Sandvik SAF 2507
Titanium (CP Ti)

1) ASTM 317L, e.g. Sandvik 3R64
2) EN 1.4439, e.g. Sandvik 3R68