このページは英語版のみです。 (This page is only available in English)

Heat exchanger tubing

Stainless steel, duplex or nickel alloy? Choosing the right heat exchanger tube

Choosing heat exchanger tubing means balancing corrosion resistance, strength, ease of fabrication and total cost of ownership. A common assumption is that once standard stainless steel fails, the only way forward is a nickel alloy.

There is an option in between. This guide compares Alleima’s Sanicro® 35 (UNS N08935) with standard austenitic stainless steels, duplex grades, 6Mo grades and nickel alloys, so you can see where Sanicro® 35 fits.

How the grades compare

Category Grade UNS Nominal composition (%)
Standard austeniticAlleima® 3R60 (316L)S3160317.5Cr-13Ni-2.6Mo
High-alloy austeniticAlleima® 2RK65 (904L)N0890420Cr-25Ni-4.5Mo-1.5Cu
Standard duplexSAF® 2205S3220522Cr-5Ni-3.2Mo-0.18N
Super duplexSAF® 2507S3275025Cr-7Ni-4.0Mo-0.3N
6Mo super austenitic6Mo gradeS3125420Cr-18Ni-6.1Mo-0.20N
Super austeniticSanicro® 35N0893527Cr-35Ni-6.5Mo-0.3N
Nickel-iron alloyAlloy 825N0882521Cr-42Ni-3.0Mo-2.0Cu
Nickel alloyAlloy 625N0662521Cr-≥58Ni-9.0Mo-3.5Nb
Nickel alloyAlloy C-276N1027616Cr-57Ni-16Mo-4.0W

Swipe the table sideways to see all columns.

Corrosion test results

Critical pitting temperature (CPT)

Modified ASTM G150, 3M MgCl2 (°C)

Sanicro® 35

110°C

Alleima 254 SMO (S31254) / 6Mo grade

67°C

Critical crevice temperature (CCT)

ASTM G150, 1M NaCl (°C)

Sanicro® 35

100°C

Alleima 254 SMO (S31254) / 6Mo grade

75°C

Values from the Alleima Sanicro® 35 datasheet. Test methods are shown under each chart title.

Where Sanicro® 35 is used

Refineries

It is used in refinery heat exchangers such as overhead condensers, and is a candidate material for ammonium chloride service.

Renewable fuels

It is suitable for several pretreatment technologies for renewable feedstock, such as used cooking oil cleanup.

Chemicals and petrochemicals

It suits chlorinated hydrocarbons, organic acids such as mixtures of formic and acetic acid, and inorganic acids such as phosphoric and sulfuric acid.

What would an upgrade mean for your lifecycle costs?

Explore the Alleima TCO calculator

Strength, stability and fabrication

01

Strength

Minimum yield strength is 425 MPa for solution-annealed tube. The extra strength can allow thinner tube walls in pressurized systems, which improves heat transfer and lowers material cost.

02

Structural stability

The grade has very high structural stability. Intermetallic phases can precipitate at temperatures above 600°C (1110°F).

03

Fabrication

It can be cold bent to tight radii. It expands into tubesheets the same way as standard austenitic stainless steels. Weldability has been verified in ASME IX testing, using Alloy 59 filler metal.

What it means for maintenance and cost

Fixing the root cause

When tubes fail because process conditions have moved past the material’s limits, upgrading the material deals with the cause rather than the symptom.

Approvals

Pressure codes

ASME Code Case 2982

Section VIII, Div. 1 and 2

ASME Code Case 3089

Section I

TÜV Particular Material Appraisal

Pre-approved

Questions to ask before you specify

1

How often do the current tubes fail, and what is the main corrosion mechanism?

2

Have operating conditions (temperature, pH, chlorides, H2S) changed since the unit was commissioned?

3

Can your fabricator weld, bend and expand the alloy using established procedures?

4

Could a super-austenitic grade with PREN of about 52 meet the corrosion requirements before you move to a nickel alloy?

5

Is the material approved under the pressure codes you work to (ASME, PED)?

Next steps

Find out where Sanicro® 35 fits in your unit

Talk to Alleima about your application. Our sales manager will put you in touch with the right materials specialist.

Your Alleima contact

Dwayne Tang

Sales Manager, Tube APAC Sales